Analysis of Hydroxyl Value of Polypropylene Glycol Using the PLS Method in Near-Infrared Spectroscopy
The NIR for oil and fat substances is promising when applied in the quantitation of acid value, hydroxyl value, saponification value, ester value, etc. This issue introduces examples of the quantification of the hydroxyl value of polypropylene glycol.