Relationship Between Particle Size Distribution/Particle Shape and Optical Properties of Gold Nanoparticles
We examined the particle size distribution of gold nanoparticles using the SALD-7500nano nano particle size analyzer and observed the shape of gold nanoparticles using the SPM-9700HT scannig pribe microscope. We also observed the optical properties caused by differences in the size and shape of gole nanoparticles using the UV-2700 UV-Vis spectrophotometer.