Product

Industrial Equipment

Liquid crystal injection systems

Liquid Crystal Injection for FLC Panel

ALIS-100F

LIQUID CRYSTAL INJECTION SYSTEM

ALIS-100F

"LIQUID CRYSTAL INJECTION" takes charge of important process which injects "LIQUID CRYSTAL" into an "Aligned Panels" at assembly process of liquid crystal panel.
As panel size becomes larger, further improvement for shortening an operation cycle and down sizing of equipment are being required.
It is also required to facilitate equipment to meet with customer's individual specification for their crystal implanting conditions.

SHIMADZU is producing highly qualified "LIQUID CRYSTAL INJECTION" applying these customer's requests.

Fine Temperature Control Technology

  • Temperature distribution in the cell 130 ± 1.5°C (for 17"panel)
    ‚‚Þapplying for FLC, AFLC panel etc.
  • Heating control for the crystal
    Þshortening an injection speed

Fine control technology for vacuum and pressure

  • Injection chamber is controlled precisely from high vacuum
    (10-5 Pa order) to a pressure condition (1kg/cm2G).
  • Adopting an oil-free exhausting system (Turbo-molecular pump and Dry pump)
    Þpreventing an impurity intrusion
    Þshortening an injection speed

Application technology for particle and contamination

  • Electro-polishing for an inner face of injection chamber and parts finishing
  • Adopting a slow exhausting and venting
    Þpreventing dust blown up

Auto-processing technology

  • Recipe setting suitable for various panels
  • Capability for auto systems like cassette-to-cassette

Specification;

  1. Operation speed:
    60 panels/batch for 17" panel
    (ex; 20 panels/hour as 1batch=4hours)
  2. Vacuum pumping system:
    Turbo-molecular pump + Dry pump
  3. Chamber construction: Two rooms

  • Injection chamber:
    Controlling the panel temperature (up to 130°C), it operates vacuum pumping and injection by pressure (max. 3kg/cm2G).
  • Degassing chamber:
    Controlling the temperature (up to 130°C) of the liquid crystal, it operates vacuum pumping. As it facilitate moving system of the liquid crystal tray, the tray is loaded into the injection chamber after degassing.



This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.