12.Coatings

Reflectance of Aℓ, Aℓ+MgF2, and Au

Fig. 9 Reflectance of Aℓ, Aℓ+MgF2, and Au

The energy in the diffracted light varies with the grating's coating material. It is necessary to use the coating material that is appropriate for the required wavelength. Fig. 9 shows the reflectance characteristics for Aℓ , Aℓ+MgF2, and Au.