Product

Optical and Laser Devices

Precision Spectormeters

GM-1D

NEW!! Stringent Angular Measurements and Precise Refractive Index Measurements!

GM-1D

Features

The high-accuracy encoder achieves ±1" angular measurement accuracy and ±0.00001 refractive index measurement accuracy. The angle measured by the encoder is directly displayed on a digital counter. High-accuracy ball bearings used for all rotary sliding parts ensure smooth and accurate rotation. The color-corrected objective lens eliminates the need for readjustment when the measurement wavelength changes.

Applications

Precise angle measurements for prisms, etc.
Refractive index measurements for transparent materials, such as glass.

Specifications

Measurement accuracy Angular measurement accuracy: ±1"
Refractive index measurement accuracy: ±0.00001
Display Angle counter digital display
Measurement wavelength range 404.7 nm to 706.5 nm
Slit Max. effective blade length: 15 mm
Min. reading: 0.005 mm
Objective lens Focal distance: 450 mm
Brightness: F/10
Effective diameter: 15 mm
Eyepiece lens Autocollimation eyepiece lens
Focal distance: 15 mm
Angle detector High-accuracy rotary encoder
External output RS-232C (for PC connection)
Optional refractive index calculation software
Light source Standard: Hg light source (with starter)
Optional: 30 W automatic spectrum light-source unit - Hg, He, H2, Cd.
Size and weight 1210 x 550 x 650 mm, 100 kg

The system can be customized to your requirements. Consult your Shimadzu representative.



This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.