Process 1: Forming transparent conducting film
Evaluation method / Instrument required:
Process 2: Titanium oxide paste printing and firing
Evaluation method / Instrument required:
Process 3: Soaking in solution containing dye to absorb dye in nano-scale titanium oxide structure
Evaluation method / Instrument required:
Process 4: Forming spacer
Evaluation method / Instrument required:
Process 5: Arrange catalyst electrode (platinum) against a separately formed substrate
Evaluation method / Instrument required:
Process 6: Injecting electrolyte
Evaluation method / Instrument required: