IG-1000
Measurement Principle Induced grating (IG) method
Measurement Range 0.5 to 200 nm
Measurement Time 30 sec (from the start of measurement to the display of results)
Sample Liquid Volume 250 to 300 µL
Measurement Unit Light Source Semiconductor laser (wavelength: 785 nm; output: 3 mW)
Light-receiving Unit Photodiode
Cell Batch cell (material: Pyrex glass*1)
Output Terminal Serial output (connector type: D-Sub, 25 pin, female)
Temperature Setting Range 7°C to 40°C (cell holder temperature setting range*2)
Operating Environment Temperature: 15°C to 35°C
Humidity: 20% to 80% (without condensation) Humidity: 20% to 80% (without condensation)
Power Supply AC 115 or 230 V ±10%
Size and Weight 600 (W) x 400 (D) x 200 (H) mm, approx. 15 kg

*1: Do not use the kind of solvents that may damage Pyrex glass.
* : Measurement is possible as long as the conductivity of the sample liquid does not exceed 400 μS/cm (microsiemens per centimeter). (For example, saline and seawater cannot be used for measurement unless they are greatly diluted.)

Parts Required for Installation

Micropipette "Required to inject samples into the cell. Provide a micropipette that can measure out 200 µL with an accuracy of 5%."

* Sold by Shimadzu as a special accessory and can therefore be ordered from Shimadzu if necessary.