Shim-pack Bio Series

Shim-pack Bio Diol : Size Exclusion Chromatography Columns

With different pore sizes, Shim-pack Bio Diol LC columns are effective for analysis of aggregates and fragments of mAb, oligonucleotides and carbohydrates.

 
Shim-pack Bio Diol Diol-60 Diol-120 Diol-200 Diol-300
Particle Silica
Ligand Dihydroxypropyl(Diol)
Particle Size 3 μm,5 μm 2 μm,3 μm,5 μm
Pore Size 6 nm 12 nm 20 nm 30 nm
pH Range 5.0 - 7.5
Molecular
Weight Range
below 10,000 1,000 - 100,000 5,000 - 300,000 20,000 - 1,000,000
 

Shim-pack Bio IEX : Ion Exchange Chromatography Columns

Shim-pack Bio IEX Columns are available in Q (quaternary ammonium) and SP (sulfopropyl) chemistries and are based on porous (Q and SP columns) and non-porous (Q-NP and SP-NP columns) hydrophilic polymers with low nonspecific adsorption. The porous particles offer excellent binding capacity with exceptionally high efficiency and the non-porous particles offer high efficiency and exceptional resolution.

Analysis of Synthesized Oligonucleotide (Single Strand DNA) using Shim-pack BIO IEX Q-NP

 
Shim-pack Bio IEX Q-NP SP-NP Q SP
Particle hydrophilic non-porous polymer hydrophilic non-porous polymer
Particle Size 3 μm,5 μm 5 μm
Ligand -CH2N+(CH3)3 -(CH2)3SO3- -CH2N+(CH3)3 -(CH2)3SO3-
pH Range 2 - 12

Shim-pack Bio HIC:Hydrophobic Interaction Chromatography

Shim-pack Bio HIC Column is a hydrophobic interaction chromatography (HIC) column packed with butyl bonded hydrophilic nonporous polymer particles (4μm). HIC is suitable for the separation of anlaytes with slightly different hydrophobicity, such as antibody-drug conjugate (ADC) with different drug-antibody ratios (DAR). Shim-pack Bio HIC can be used for the analysis of DAR of ADC with relatively low pressure and high resolution.



 

Order Information

  Shim-pack Bio HIC
Particle Size 4 µm
4.6 x 100mm 227-31174-01
 

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.