Shim-pack ISC Series

HPLC Column Solutions

Shim-pack ISC series uses polystyrene gel as solid support, making it possible to utilize both electrostatic reaction and hydrophobic reaction. Shim-pack ISC-05 is suitable for the analysis of guanidine compounds.

For applications, please click here.

Column Stationary
phase
Particle
Size
(µm)
Dimensions
(I.D. x Length, mm)
P/N Guard
Column
Shim-pack
ISC-05/S
0504
Na type
sulfone group
5 4.6 x 38 228-09700-91 228-00802-91
Shim-pack
ISC-07/S
1504
Na type
sulfone group
7 4.0 x 150 228-09328-91
Shim-pack
ISC-07/S
1504 Li
Li type
sulfone group
7 4.0 x 150 228-00796-91 228-00797-91

Brochure download

Download the latest brochure.

Brochure 

For Research Use Only. Not for use in diagnostic procedures.