Shim-pack VP Series

HPLC Column Solutions

Strict Manufacturing Uniformity

Comparison of reproducibility between three batches of silica-based materials

Balance of Number of Theoretical Plates and Column Pressure

Shim-pack VP series achieves a higher number of theoretical plates while maintaining low pressure. It provides superior performance shown by NTP per 1MPa.

NTP per 1MPa
Column Size: 4.6 x 150 mm, Mobile Phase: Methanol/Water=70/30,
Flow Rate: 1.0 mL/min., Sample: Naphthalene

Excellent Peak Shape

Packing materials with less metal impurities achieve excellent peak shape of coordination compounds.

Completed end-capping achieves excellent peak shape of basic compounds.

Smooth Transfer of Methods from High-Speed Analysis to Conventional Analysis

By using the Shim-pack VP series of conventional columns in combination with the Shim-pack XR series of high-speed columns, which offer the equivalent separation performance, it is possible to perform method development via high-speed analysis, and then smoothly transfer to conventional analysis. Utilizing these columns with Nexera Method Scouting provides strong support for method development.

Conditions
Column Top:
Shim-pack VP-ODS
(150 mmL. × 4.6 mmI.D., 5 μm)
(P/N: 228-34937-91)
    Bottom:
Shim-pack XR-ODS
(50 mmL. × 3.0 mmI.D., 2.2 μm)
(P/N: 228-41606-92)
Mobile Phase A) 0.1 % formic acid
B) Acetonitrile
A/B = 8/2 (v/v)
Flow Rate Top: 1.0 mL/min
Bottom: 1.0 mL/min
 
 
 

Relative Retention Times

Peak Shim-pack VP-C8 Shim-pack XR-C8
  1. Sulfadiamine 1.000 1.000
  2. Sulfamerazine 1.252 1.238
 3. Sulfadimidine 1.537 1.509
 4. Sulfamethoxazole 2.809 2.699
 5. Sulfaquinoxaline 5.668 5.432

Analysis of Fat-Soluble Vitamin

Conditions
Column Top:
Shim-pack VP-C8
(150 mmL. × 4.6 mmI.D., 5 μm)
(P/N: 228-59927-91)
  Bottom:
Shim-pack XR-C8
(50 mmL. × 3.0 mmI.D., 2.2 μm)
(P/N: 228-59902-92)
Mobile Phase Methanol
Flow Rate Top: 1.0 mL/min
Bottom: 1.0 mL/min
 

Relative Retention Times

Peak Shim-pack VP-C8 Shim-pack XR-C8
1. Retinol 1.000 1.000
2. α±−tocopherol 1.509 1.531


 

 
 

Analysis of Fat-Soluble Vitamin

Conditions
Column Top:
Shim-pack VP-C8
(150 mmL. × 4.6 mmI.D., 5 μm)
(P/N: 228-59927-91)
  Bottom:
Shim-pack XR-C8
(50 mmL. × 3.0 mmI.D., 2.2 μm)
(P/N: 228-59902-92)
Mobile Phase Methanol
Flow Rate Top: 1.0 mL/min
Bottom: 1.0 mL/min

 

Relative Retention Times

Peak Shim-pack VP-C8 Shim-pack XR-C8
1. Retinol 1.000 1.000
2. α±−tocopherol 1.509 1.531
 

Batch Analysis of Non-Steroidal Anti-Inflammatory Drugs (NSAIDs)

Conditions
Column Top:
Shim-pack VP-Phenyl
(150 mmL. × 4.6 mmI.D., 5 μm)
(P/N: 228-59928-91)
  Bottom:
Shim-pack XR-Phenyl
(50 mmL. × 3.0 mmI.D., 2.2 μm)
(P/N: 228-59904-92)
Mobile Phase A) 20 mmol/L Phosphoric acid (Na) buffer (pH 2.5)
B) Acetonitrile
A/B = 3/7 (v/v)
Flow Rate Top: 1.0 mL/min
Bottom: 1.0 mL/min

 

Relative Retention Times

Peak Shim-pack VP-Phenyl Shim-pack XR-Phenyl
1. Piroxicam 1.000 1.000
2. Ketoprofen 1.480 1.483
3. Diflunisal 2.233 2.172
4. Diclofenac 2.949 2.916
5. Indomethacin 3.263 3.262
6. Ibuprofen 3.470 3.501

Specifications

  Shim-pack VP-ODS Shim-pack VP-C8 Shim-pack VP-Phenyl
 Particle Size (µm)  5  5  5
 Pore Size (nm)  12  12  12
 Surface Area (m2/g)  410  410  410
 Carbon Loading  20%  12.5%  12.3%
 Pressure Tolerance (MPa)  Approx. 20  Approx. 20  Approx. 20
 Pore Volume (mL/g)  1.25  1.25  1.25
 End-capping  Yes  Yes  Yes
 Bonding Type  Monomeric  Monomeric  Monomeric
 pH range  2-7.5  2-7.5  2-7.5
 USP Code  L1  L7  L11

* Appearance and specifications are subject to change without notice.

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page