Refractive Index Detector

RID-20A

Specifications

RID-20A
 Refractive index range  1 to 1.75 RIU  Maximum operating flow rate  20 mL/min (150 mL/min with option
 Noise level  2.5 ×10-9 RIU max  Temperature control of cell unit  30 to 60 ℃
 Drift  1×10-7 RIU/h max  Cell volume  9 μL
 Range
 A mode: 0.01 × 10-6 to 500 × 10-6 RIU
 P and L mode: 1 × 10-6 to 5,000 × 10-6 RIU
 Cell withstand pressure  2 MPa (cell unit)
 Response  0.05 to 10 sec, 10 steps Operating temperature range  4 to 35 ℃
 Polarity switching   SupportedDimensions, weight  Dimensions, weight  W260 × D420 × H140 mm, 12 kg
 Zero adjustment  Auto zero, optical zero,  fine zero  Power requirements  AC 110 V, 230 V, 150VA, 50/60 Hz

Please contact representative if you need Hexafluoroisopropanol(HFIP)  as the mobile phase.

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page