X-ray fluoroscopy systems offer non-destructive observations of the internal structures of objects. They are effective instruments for identifying the cause of failure of industrial products.

By simplifying the non-destructive tomographic imaging and 3D imaging of the interior of objects, observations of internal shapes, dimensional measurements, and density observations, these systems are powerful tools for defect analysis and quality control.

These are images of the electrodes and separators on an arbitrary cross-section.

Internal Observations of Electrodes and Separators (X-ray CT)

inspeXio SMX-225CT Microfocus X-ray CT System

inspeXio SMX-225CT Microfocus X-ray CT System

Industrial X-ray CT systems offer non-destructive internal observations of objects. A CT system with submicron-level resolution is effective for clearly identifying the internal status of complex electronic components. These systems are employed for final quality control in the battery production process.

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page