X-Ray Fluorescence Analysis of Residual Catalysts

Many familiar industrial products are made of organic compounds and their manufacturing processes involve various synthesis reactions and metal catalysts. Catalysts are mainly divided into two categories: homogeneous catalysts and heterogeneous catalysts. In general, homogeneous catalysts are used for manufacturing pharmaceuticals and chemicals. While the reactions of homogeneous catalysts can be controlled rigorously, separation of reaction products is difficult.
Meanwhile, there is a need to control the amount of residual catalysts in terms of the safety of the products and the re-use of expensive catalysts. For example, the Guideline for Elemental Impurities (ICH Q3D) enforced in April 2017 requires a risk assessment for substances, such as catalysts, that are purposely added during the manufacturing process.
This article introduces an example analysis of the amount of residual homogeneous catalyst following a synthesis reaction using the Pharmaceuticals Impurities Screening Method Package; in this example we used palladium (Pd), a substance widely used as a catalyst, for a cross-coupling reaction which is widely used for the synthesis of organic compounds.

t1_calibration

t2_results

t3_conditions

 
 

EDX-7000/8000/8100

EDX

Features: 

Energy Dispersive X-ray Fluorescence Spectrometer
The EDX-8100 offers enhanced versatility with the ability to analyze even light elements in liquid samples with high sensitivity by helium purging.

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page