Measurement of Sodium and Potassium in Portland Cement by Flame Atomic Absorption Method

Here, using flame atomic absorption method, we introduce an example of analysis of Na and K in a standard sample of Portland cement (211R) obtained from the Japan Cement Association to determine their respective concentrations.