Since EDX can analyze a sample regardless of its size or shape, irregular objects such as glassbottles or their broken pieces and laser disc plates can be easily analyzed. In addition, traceelements in glass can be detected using a Zr filter. Shown below are examples of qualitative andquantitative analysis of borosilicate glass and qualitative analysis of trace elements within specialglass.