EDXRF Analysis of Lead, Cadmium, Mercury and Chromium in Zinc Alloy

X-ray fluorescence analysis can be used to quicklyand easily analyze samples in solid, powder and liquid states nondestructively, and is therefore widely used as a screening method for compliance with the RoHS/ELV directives. Here we present the results of our evaluation of the calibration curves for Pb, Cd, Hg and Cr in MBH-manufactured Zn alloy reference materials, as well as our evaluation of the analysis sensitivity.