Comparison of Calibration Curves of Lead, Cadmium and Chromium in Zinc Alloy and Copper Alloy

X-ray fluorescence analysis allows for the nondestructiveanalysis of solid, powder and liquidsamples, both quickly and easily. For that reason it iswidely used as a screening method for RoHS/ELVcompliance testing.In this Application News, we compared the calibrationcurves for Zn alloy and Cu alloy, and present ourexamination of their applicable ranges.