Screening Analysis of Brominated Flame Retardants with ATR Accessory (1) (RoHS Directive)

We introduce here an example of screening analysis for brominated flame retardant using the single reflection ATR accessory provided with the FTIR spectrophotometer.

Content Type:
Application
Document Number:
LAAN-A-FT-E003
Product Type:
Molecular Spectroscopy, FTIR Spectroscopy
Keywords:
ATR, Electronics, Electronic, Semi-conductor, Electronic parts, Mounting board, Printed Circuit Board, DuraSampⅡRⅡ