Points to Consider with Respect to ATR Spectra of Inorganic Compounds

It is widely known that ATR spectra obtained using the ATR measurement method have a different peak intensity ratio than peaks collected using transmission measurement. This Application News introduces points to consider with respect to ATR spectra of inorganic compounds.