Investigation of Additives in Plastics by FTIR-ATR Spectroscopy

Commercially available plastic products contain polymers, such as polyethylene (PE) and polypropylene (PP), as their main components, in addition to various trace components that are added to enhance
performance and maintain quality.
Here we introduce an evaluation of additives used in plastic bags taking advantage of the high S/N ratio of the Shimadzu FTIR IRTracer-100 spectrophotometer.

Content Type:
Application
Document Number:
LAAN-A-FT-E051
Product Type:
Molecular Spectroscopy, FTIR Spectroscopy
Keywords:
Plastics, polyethylene, polypropylene, Hydrocarbon Processing Industry (Petrochemical, Chemical), Petrochemical, Polymer, Rubber, Resin, Plastics, IRTracer-100
Language:
English
File Name:
jpa213019.pdf
File Size:
1,836kb

Free Download

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page