Identification of Contaminant Found in Resin Production Process Using IR Pilot
The Shimadzu IRSpirit launched recently is a compact Fourier transform infrared spectrophotometer characterized by the highest signal to noise ratio and the highest maximum resolution in its class.
This article introduces the contaminant analysis using the IR Pilot.