Determination of Volatile Organic Compounds in Water-based Paints and Varnishes Using Gas Chromatography
In lieu of the recent development and demand for the analysis of paints ad varnishes with low content of Volatile Organic Compounds (VOCs), a fast and efficient using the Gas Chromatography (with Flame Ionization Detector) was developed to determine the amount of VOCs. This method was optimized based on GB 18582-2008. The method takes into account the quantitation of 30 VOCs commonly found in paint. Precision of system was illustrated by excellent repeatability of the results obtained.