Fast Analysis of Acrylonitrile in ABS Polymer Using a Backflush GC System

Residual organic solvent in food packaging materialsis a problem that receives serious attention because ofthe implications to food safety and public assurance.While food containers and packaging materials aresubject to standards controlled through materialtesting and testing of leachates from the packagingmaterials, as specified in Japan’s Food Sanitation Law,the recent heightened concern over safety andassurance has led to the analysis of substances otherthan those subject to the current control standards inJapan. One example of these is the measurement ofacrylonitrile, which is controlled as a carcinogen by theU.S. Food and Drug Administration (FDA) and byregulations in the European Union (EU).This Application News introduces a fast analysis ofacrylonitrile based on the use of the backflush GCsystem.

Content Type:
Application
Document Number:
LAAN-A-GC-E030
Product Type:
Gas Chromatography
Keywords:
Hydrocarbon Processing Industry (Petrochemical, Chemical), Rubber, Resin, Plastics, Backflush GC System
Language:
English
File Name:
g264.pdf
File Size:
1,276kb

Free Download

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page