Analysis of Vinyl Chloride in Polyvinyl Chloride Plastics by Headspace Gas Chromatography with a Flame Ionization Detector (GC/FID)

The 16th revision of the Japanese Pharmacopeia was announced in the Japanese Ministry of Health, Labour and Welfare Notification No. 65 dated March 24, 2011, and its use became effective as of April 1, 2011. In this revision, under the Test Methods for Plastic Containers, the headspace GC/FID method has been adopted as the test method for vinyl chloride in polyvinyl chloride injection containers used for aqueous solutions.This Application News describes the test method for analysis of vinyl chloride contaminants in polyvinyl chloride injection containers used for aqueous solutions as specified in the 16th revision of the Japanese Pharmacopeia.

Content Type:
Application
Document Number:
LAAN-A-GC-E042
Product Type:
Gas Chromatography
Keywords:
Polyvinyl Chloride, Vinyl chloride, Hydrocarbon Processing Industry (Petrochemical, Chemical), Pharmaceutical, Life Science, Rubber, Resin, Plastics, TruboMatrix HS-40 (short transfer), GC-2010 Plus AF
Language:
English
File Name:
jpc112005.pdf
File Size:
987kb

Free Download

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page