Analysis of Gas Generated from Lithium Ion Rechargeable Battery Cells
Electrolytic solutions in lithium ion rechargeable batteries consist of organic solvents (mainly composed of the carbonate series), electrolytes, and additives.GC-MS systems are effective for the analysis of the denatured components of electrolytic solutions resulting from the charging and discharging of batteries. This article introduces a sample analysis of gas produced from a lithium ion rechargeable battery cell stored for 5 days at 80 ℃ cold areas like Hokkaido and hot areas like Okinawa.
- Content Type:
- Application
- Document Number:
- LAAN-J-MS-E022
- Product Type:
- Mass Spectrometry, Gas Chromatograph-Mass Spectrometry
- Keywords:
- Electrolytic solutions, Electronics, Electronic, Automotive, Li-ion Battery, GCMS-QP2010 Ultra
- Language:
- English
- File Name:
- jpo212077.pdf
- File Size:
- 213kb