Inner Observation of Aluminum Die Casting Parts

X-ray fluoroscopy systems have been widely used to detectblowholes, porosities, cracks, and other internal defects inaluminum die cast products.In recent years however, with increased miniaturization anddensity of machine components, detailed information onsuch defects including positioning, shape, and size isincreasingly demanded, and detailed 3 dimensionalobservations have become essential.As a means of responding to such demands, this paperintroduces examples of the observation of internal defectsin aluminum die cast parts using an X-ray CT system.The inspeXio SMX-225CT microfocus X-ray CT systemwas used to obtain the images.

Content Type:
Application
Document Number:
LAAN-A-ND-E001
Product Type:
Non-Destructive Testing
Keywords:
Electronics, Electronic, Engineering Materials, inspeXio SMX-225CT
Language:
English
File Name:
n112.pdf
File Size:
241kb

View Article

For Research Use Only. Not for use in diagnostic procedures.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

Top of This Page