Analysis of Phosphate Ester Adsorption Film Formed on Surface of Iron Oxide in Lubricant by SPM-8100FM
The SPM-8100FM is capable of analyzing the lubricant-iron oxide interface with molecular resolution from a lubricant sample of only 500 μl. Because the performance of lubricants can be evaluated by a laboratory-scale material test, this instrument is expected to provide a new evaluation technique that substantially reduces costs related to lubricant development.