Analysis of Resin Using FTIR and Thermal Analysis - "Silent Change" -
The act of part and material suppliers changing the composition of parts and materials without gaining the approval of their clients is known as "silent change". This article introduces an example analysis of a case in which the material of a gear was changed.
- Content Type:
- Application
- Document Number:
- LAAN-A-TA-E018
- Product Type:
- Thermal Analysis
- Keywords:
- FTIR, DSC, POM, Homopolymer, Copolymer, Crystalline, Amorphous, PET, Hydrocarbon Processing Industry (Petrochemical, Chemical), Rubber, Resin, Plastics, DTA
- Language:
- English
- File Name:
- jpc318008.pdf
- File Size:
- 149kb