Tensile Testing of Cultured Epidermis
In this research, tensile tests were performed using cultured epidermis, which is a regenerative medical product, and milk membrane imitating cultured epidermis (collected from the surface of hot milk) as an example of a quantitative evaluation of a material's mechanical properties.