Tensile Test of Metallic Material by Strain Rate Control Using a Strain Gauge Extensometer
In the revisions of the standards ISO 6892/JIS Z 2241 for tensile testing of metallic materials, strain rate control (measurement of strain with an extensometer) was added as a test item in addition to the conventional stress rate control as a method for loading materials to their yield point.
In this experiment, measurements of the elastic modulus of a metallic material was carried out by strain rate control using a Shimadzu SSG-H strain gauge extensometer, demonstrating that testing which amply satisfies the specified strain rate tolerance of ±20% is possible with this device.
- Content Type:
- Application
- Document Number:
- i276
- Product Type:
- Materials Testing & Inspection, Universal / Tensile Testing Machine
- Keywords:
- Metal, tensile test, extensometer, JIS, ISO, strain control, predicted strain control, fracture point, elastic modulus, strain gauge, SSG-H, Hydrocarbon Processing Industry (Petrochemical, Chemical), AGX-100kNV
- Language:
- English
- File Name:
- jpi320007.pdf
- File Size:
- 610kb