Detection of Inclusions in Metal Materials Using an Ultrasonic Fatigue Testing System
In this experiment, we performed the detection of inclusions in an SNCM439 specimen using the ultrasonic fatigue testing system, USF-2000A, and observed the inclusions using the electron probe micro analyzer, EPMA, to identify their elements.