The Assessment of Dissolution Process of Powdered Sports Drink by Continuous Measurement Function of SALD Series
In this research, taking a powdered sports drink as a sample, we measured the particle size distribution in the dry state, and the change in particle size distribution as the sample dissolves after being added to water, using the SALD series laser diffraction particle size analyzer.