Observing the Failure of Open-Hole CFRP specimens in Tensile Tests-Synchronized Imaging Using Two High-Speed Video Cameras-
It is important to confirm the failure process of weak regions, such as the periphery of circular holes, for CFRP development and to confirm the validity of CAE analysis. However, since the failure of open-hole CFRP is a brittle phenomenon, where failure occurs instantaneously, it cannot be confirmed with the naked eye. For this reason, high-speed video cameras are used to observe the failure of CFRP. In this experiment, synchronized images were obtained at the front and the side of the specimens using two HPV-X2 high-speed video cameras.
- Content Type:
- Application
- Document Number:
- LAAN-A-HV-E004
- Product Type:
- Materials Testing & Inspection, High-Speed Video Camera
- Keywords:
- Open-hole CFRP, Static tensile testing, High-speed video camera, Fracture observation, Synchronized images, Hydrocarbon Processing Industry (Petrochemical, Chemical), Rubber, Resin, Plastics, HPV-X2
- Language:
- English
- File Name:
- jpi715002.pdf
- File Size:
- 2,755kb