Aluminum Die Castings

Defect analysis identifies voids and displays a color-coded map of the voids based on their volume. It can also display a frequency histogram of scale the void volume and count.

By scanning the die cast part before machining and then specifying the surface after machining (CAD data), the software can determine which voids are removed by machining, which remain internally, and which are exposed on the surface after machining.

Voids that are removed
Internal voids
Voids exposed on the surface

GFRP(Glass Fiber Reinforced Plastic)

 

CFRTP (Continuous Fiber Reinforced Thermoplastic Laminate)

Provided by Ehime University

BGA (Ball Grid Array)

Concrete

Lithium-Ion Rechargeable Battery

Rectangular Lithium Polymer Battery (for Smartphones)

Circuit Board


MPR Image FOV = ø 4.4 mm

Mouse fetus


MPR Image FOV = ø 13.7 mm

Analysis Using PointMaster Reverse Engineering Software

The software can align CT data with 3D-CAD data, calculate the distance between the boundary surface defined in the CT data and the corresponding 3D-CAD data, and display a color-coded map based on such differences.