inspeXio SMX-225CT FPD HR Plus

Microfocus X-Ray CT System

Applications 1

Aluminum Die Castings

Defect analysis identifies voids and displays a color-coded map of the voids based on their volume. It can also display a frequency histogram of scale the void volume and count.

By scanning the die cast part before machining and then specifying the surface after machining (CAD data), the software can determine which voids are removed by machining, which remain internally, and which are exposed on the surface after machining.

Voids that are removed
Internal voids
Voids exposed on the surface