Chemical compatibility chart

  Sample solution for Ion chromatography
Acid 10% acetic acid solution ✓
30% acetic acid solution ✓
Hydrochloric acid ✓
Nitric acid  
Sulfuric acid  
Alkali 1.0 M potassium hydroxide solution (KOH) ✓
3.0 M potassium hydroxide solution (KOH) ✓
1.0 M sodium hydroxide solution (NaOH) ✓
3.0 M sodium hydroxide solution (NaOH) ✓
Alcohol Methanol ✓
Ethanol ✓
1-Propanol (n-propanol) ✓
Isopropanol (2-propanol) ✓
1-Butanol (n-butanol) ✓
1-Pentanol (n-pentanol) ✓
Ethylene glycol (ethane-1,2-diol) ✓
Propylene glycol (1,2-propanediol) ✓
Glycerol (glycerin) ✓
Others Acetonitrile  
N,N-Dimethylformamide (DMF)  
Dimethyl sulfoxide (DMSO)  
{"title":"Specification Sheet Downloads","description":"Download the latest specification sheets.","source":"product","key":5841,"max":30,"filter_types":["spec_sheet"],"link_title":"View other Downloads","link_url":""} {"title":"Downloads","description":"Download the latest brochure.","source":"product","key":5841,"max":30,"filter_types":["brochures"],"link_title":"View other Downloads","link_url":"","pdf_links":[]}