Testing Machine for Rubber Vibration Isolators

Maximum test force

±10kN

Maximum displacement

±10mm

Cycle speed

5 to 300 Hz

Amplitude Characteristics

50Hz ±2mm ,100Hz ±0.9mm , 200Hz ±0.36mm , 300Hz ±0.18mm