HMV-G Series - Specs

Micro Vickers Hardness Testers

HMV-G31S

Monochrome Camera without Electric Turret

HMV-G31 Series

Model P/N

344-04273-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G30DT

Monochrome Camera with Electric Turret

HMV-G30 Series

Model P/N

344-04276-□□

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Thermal printer
Compatible with laser printers

External Output : USB

Transfer of test results to a USB flash drive (CSV format)

Results Displayed : Graphical Display

Variance graph, histogram, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Effective Measurement Range
(For 40× objective lens)

250×250μm

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Eyepiece

×10

Indentation Reading System

Manual readings via an optical microscope

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2× (1 empty)

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31-XY-S-HC

Color Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04293-□□

Autofocus Function

N

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G31-FA-D-HC

Color Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04292-□□

Autofocus Function

Y

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (Super-long
Working Distanse)
5× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G31-FA-S-HC

Color Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04291-□□

Autofocus Function

Y

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (Super-longWorking Distanse)
5× (0 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G31-XY-D

Monochrome Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04282-□□

Autofocus Function

N

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G31-XY-S

Monochrome Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04281-□□

Autofocus Function

N

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G31-FA-D

Monochrome Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04280-□□

Autofocus Function

Y

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (Super-long
Working Distanse)
5× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G31-FA-S

Monochrome Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04279-□□

Autofocus Function

Y

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (Super-longWorking Distanse)
5× (0 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less

HMV-G Series

Test force rang

0.0098 to 19.6 N

Reading method

Automatic (G31) Manual (G30)

Maximum number of indenters and object lenses installed

S: Indenters 1, Object lenses 2
D: Indenters 2, Object lenses 4

With electrically driven revolver

HMV-G31ST/G31DT

Read more
Show Less

HMV-G30D

Monochrome Camera without Electric Turret

HMV-G30 Series

Model P/N

344-04272-□□

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Thermal printer
Compatible with laser printers

External Output : USB

Transfer of test results to a USB flash drive (CSV format)

Results Displayed : Graphical Display

Variance graph, histogram, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Effective Measurement Range
(For 40× objective lens)

250×250μm

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages*1

Eyepiece

×10

Indentation Reading System

Manual readings via an optical microscope

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2× (1 empty)

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31ST

Monochrome Camera with Electric Turret

HMV-G31 Series

Model P/N

344-04277-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Port*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G30ST

Monochrome Camera with Electric Turret

HMV-G30 Series

Model P/N

344-04275-□□

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Thermal printer
Compatible with laser printers

External Output : USB

Transfer of test results to a USB flash drive (CSV format)

Results Displayed : Graphical Display

Variance graph, histogram, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Effective Measurement Range
(For 40× objective lens)

250×250μm

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Eyepiece

×10

Indentation Reading System

Manual readings via an optical microscope

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G30S

Monochrome Camera without Electric Turret

HMV-G30 Series

Model P/N

344-04271-□□

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Thermal printer
Compatible with laser printers

External Output : USB

Transfer of test results to a USB flash drive (CSV format)

Results Displayed : Graphical Display

Variance graph, histogram, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Effective Measurement Range
(For 40× objective lens)

250×250μm

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Eyepiece

×10

Indentation Reading System

Manual readings via an optical microscope

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31DT-HC

Color Camera with Electric Turret

HMV-G31 Series

Model P/N

344-04290-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2× (1 empty)

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31D-HC

Color Camera without Electric Turret

HMV-G31 Series

Model P/N

344-04288-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2× (1 empty)

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31DT

Monochrome Camera with Electric Turret

HMV-G31 Series

Model P/N

344-04278-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages*1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2× (1 empty)

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31D

Monochrome Camera without Electric Turret

HMV-G31 Series

Model P/N

344-04274-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2× (1 empty)

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31ST-HC

Color Camera with Electric Turret

HMV-G31 Series

P/N

344-04289-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31S-HC

Color Camera without Electric Turret

HMV-G31 Series

Model P/N

344-04287-□□

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 μm
Color Camera: 195 × 160 μm

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: With the HMV-G31 series, a power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 45 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4 ③ Brinell hardness: HB*4 ④ Triangular Pyramid Hardness HT*3
⑤ Length, direct reading L (μm)*5 ⑥ Fracture Toughness Kc
⑦ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

XY Stage

Area: 100 × 100 mm; Stroke: ±12.5 mm; Sample: Maximum height 100 mm
Instrument’s lateral direction (width direction): Unlimited*3;
Instrument’s depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 200 mm max.*3
Z Axis Stroke: 60 mm; Spacer provided: Thickness 40 mm; Maximum Loading: 10 kg
The center of gravity of objects loaded must be located on the stage.

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis, and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× (1 empty)

Maximum Number of Objective Lens Attachments

2

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

1

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows® 10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports*8: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and
one USB 2.0 or 3.0 port

*1) An arbitrary test force can be configured in the range of 9.807 mN to 19.61 N, in increments of the minimum 9.807 mN (HV 0.001).
*2) When performing tests with the retention time set to 60 seconds or longer, turn ON the instrument at least 30 minutes before starting the test.
*3) The width of open space in the instrument’s depth direction is approximately 140 mm.When testing samples with a width of 120 mm or less and a depth of 175 mm or more, give consideration to the required movement range of the XY stage,and ensure that the width of the open space is not exceeded.Ensure that the shape of the sample is such that it is stable when placed on the XY stage.
*4) The Knoop indenter, Brinell indenter and triangular pyramidal indenter are optional. The Brinell hardness and triangular pyramidal hardness are only readin manually

Read more
Show Less

HMV-G31-XY-D-HC

Color Camera with Electric Turret

HMV-G31-FA and HMV-G31-XY (HMV-G31 + Electric XY Stage)

Model P/N

344-04294-□□

Autofocus Function

N

Power supply

Main unit: Single-phase 100 to 115 VAC, 230 VAC, 100 VA (50/60 Hz)
Motor Control Box: Single-phase 100 VAC, 100 VA (50/60 Hz)
Note: Prepare a grounded outlet. (D type ground, with a ground resistance of 100 Ω max.)
Note: A power supply for the PC will be required in addition to the above mentioned.

Weight

Approx. 50 kg

External Dimensions

Approx. W350 × D570 × H540 mm

External Output : Printer

Printer output from a PC via software

Results Displayed : Graphical Display

Variance graph, depth of hardening graph*6

Results Displayed : Displayed Items

Data No., diagonal line length, hardness, conversion value, average, standard deviation,
coefficient of variation, maximum value, minimum value, pass/fail determination

Data Processing Functions

① Vickers Hardness HV ② Knoop hardness HK*4③ Brinell hardness: HB*4④ Triangular Pyramid Hardness HT*3
⑤ Fracture Toughness Kc ⑥ Shape correction function (cylindrical surfaces and spherical surfaces)
Note: The cracks for measuring fracture toughness are determined manually by the operator.

Image Acquisition Functions

Total image acquisition function and edge detection function

Pattern Settings Items

Linear division, linear pitch, matrix, rectangular division, rectangular pitch, square, circular division,
circular pitch, arbitrary, zigzag

XY Stage

Area: 125 × 125 mm; XY Axis Stroke: ±25 mm; Sample: Maximum height 65 mm
Instrument’s lateral direction (width direction): Unlimited
Instruments depth direction: Unlimited for samples with a width of 120 mm max.*3
When sample width is greater than 120 mm: 175 mm max.
Z Axis Stroke: 45 mm; Spacer provided: Thickness 30 mm
Note: There is also a large sample stage edition with an area of 200 × 200 mm and an XY axis stroke of ±60 mm.

Test Force

16 stages in total
9.807 mN, 19.61 49.03, 98.07, 245.2, 490.3, 980.7 mN, 1.96 N, 2.942, 4.903, 9.807, 19.61 N
12 stages (HV0.001, HV0.002, HV0.005, HV0.01, 0.025, 0.05, 0.1, 0.2, 0.3, 0.5, 1, and 2)
plus four user-designated stages *1

Effective Measurement Range
(For 40× objective lens)

Monochrome Camera: 120 × 90 µm
Color Camera: 195 × 160 µm

Digital Camera : Color

USB Connection (USB 3.0 Super Speed)
2/3-inch image size
Measurement image 2448 × 2048 pixels

Digital Camera : Monochrome

USB Connection (USB 2.0)
1/3-inch image size
Measurement image 640 × 480 pixels
256 tint gradations (digital image data)

Indentation Reading System

Automatic readings via digital image analysis,
and manual settings for line length measurement in the PC window

Standard Objective Lenses Provided

40× 10× (2 empty)

Maximum Number of Objective Lens Attachments

4

Standard Indenter Provided

Vickers Indenter

Maximum Number of Indenter Attachments

2

Test Force Duration Time

User-designated settings from 0 to 999 sec*2, in 1 sec increments

Loading Unit

Automatic loading and automatic force changing

PC Provided*8

OS: Windows®10 (64 bit edition)
CPU: Intel® Core™ i5-6500 or faster
USB Ports: For monochrome camera
Uses two USB 2.0 or 3.0 ports
For color camera
Uses one USB 3.0 port (required) and one USB 2.0 or 3.0 port

*5) The direct length reading is only available with HMV-G30 series.
*6) Depth of hardening graphs can only be displayed when the digital micrometer (optionally available) is used.
*7) The set items with the PC provided by Shimadzu is recommended.
*8) Another USB 2.0 or 3.0 port must be added if using the electric micrometer kit.Connect the electric micrometer kit to a USB 2.0 port when using it with a color camera type unit.

Read more
Show Less