510

Loading Unit : Loading Method

Electromagnetic force

Indenter : Upper pressure indenter

Type: Flat indenter (50 µm diameter)
(500 µm flat indenter as option)
Material: Diamond

External Dimensions

Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

Utilities : Humidity

80% max. (no condensation)

Utilities : Vibration

Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
0.01 µm max. (at less than 10 Hz)
Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
0.005 µm max. (at less than 10 Hz)

Utilities : Temperature

Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

Utilities : Grounding*1

The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

Utilities : Power Consumption

Approx. 100 W (not including power consumption of PC)

Available test parameters : Power Supply

Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

Available test parameters : Data Processing Items

Calculation of compressive strength, display of test parameters and results
Display of test force and displacement data
Display of test force/displacement curve
Display of test force/displacement identification value
Display of strength/particle diameter curve
Display of displacement/time curve
Display of strength/parameter curve

Available test parameters : Shape of specimen

Particle, fiber or other shapes

Available test parameters : Test mode

Compression test, load-unload test, cyclic test

Specimen stage : Horizontal positioning range

25 mm for both X and Y directions
Min. increment: 0.01 mm (0.001 mm with option)

Specimen Stage : Area

Approx. W 125 mm × D 125 mm

Specimen stage : Vertical positioning range

Approx. 60 mm

Indenter : Lower pressure plate

SKS flat plate (Diamond pressure plate available as option)

Optical Head : Min. increment

0.01 µm / pulse

Loading unit : Loading range (mN)

9.8 – 4903

Optical monitor : Total magnification

Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

Loading unit : Load Accuracy

Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

Loading unit : Resolution (µm)

5 (when testing at 49 mN or less)

Displacement measurement unit : Method

Differential transformer

Displacement measurement unit : Measurement range (µm)

0 – 100

Displacement measurement unit : Min. increment (µm)

0.001

Displacement measurement unit : Linearity

Within ± 2% of full scale

Optical Monitor : Objective Lens

× 10, × 50 (× 20, × 40, × 100 with option)

Optical Head : Effective measurement range

Approx. 200 µm (with × 50 objective lens)

Optical Monitor : Eyepiece

× 10

Optical monitor : Illumination method

Epiluminescent

Optical monitor : Illumination lamp

LED 3 W / 3 V

Optical monitor : Light path

Switching between observation and photography possible

Optical Head : Collimation method

Direct connection between encorder and control handle: synchronized movement of two indexes

Optical Head : Detector

Optical encoder

Weight

Tester: Approx. 60 kg Control unit: Approx. 5 kg

*1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

Read more
Show Less

511

Loading Unit : Loading Method

Electromagnetic force

Indenter : Upper pressure indenter

Type: Flat indenter (50 µm diameter)
(500 µm flat indenter as option)
Material: Diamond

External Dimensions

Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

Utilities : Humidity

80% max. (no condensation)

Utilities : Vibration

Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
0.01 µm max. (at less than 10 Hz)
Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
0.005 µm max. (at less than 10 Hz)

Utilities : Temperature

Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

Utilities : Grounding*1

The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

Utilities : Power Consumption

Approx. 100 W (not including power consumption of PC)

Available test parameters : Power Supply

Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

Available test parameters : Data Processing Items

Calculation of compressive strength, display of test parameters and results
Display of test force and displacement data
Display of test force/displacement curve
Display of test force/displacement identification value
Display of strength/particle diameter curve
Display of displacement/time curve
Display of strength/parameter curve

Available test parameters : Shape of specimen

Particle, fiber or other shapes

Available test parameters : Test mode

Compression test, load-unload test, cyclic test

Specimen stage : Horizontal positioning range

25 mm for both X and Y directions
Min. increment: 0.01 mm (0.001 mm with option)

Specimen Stage : Area

Approx. W 125 mm × D 125 mm

Specimen stage : Vertical positioning range

Approx. 60 mm

Indenter : Lower pressure plate

SKS flat plate (Diamond pressure plate available as option)

Optical Head : Min. increment

0.01 µm / pulse

Loading unit : Loading range (mN)

9.8 – 4903

Optical monitor : Total magnification

Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

Loading unit : Load Accuracy

Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

Loading unit : Resolution (µm)

5 (when testing at 49 mN or less)

Displacement measurement unit : Method

Differential transformer

Displacement measurement unit : Measurement range (µm)

0 – 10

Displacement measurement unit : Min. increment (µm)

0.0001

Displacement measurement unit : Linearity

Within ± 2% of full scale

Optical Monitor : Objective Lens

× 10, × 50 (× 20, × 40, × 100 with option)

Optical Head : Effective measurement range

Approx. 200 µm (with × 50 objective lens)

Optical Monitor : Eyepiece

× 10

Optical monitor : Illumination method

Epiluminescent

Optical monitor : Illumination lamp

LED 3 W / 3 V

Optical monitor : Light path

Switching between observation and photography possible

Optical Head : Collimation method

Direct connection between encorder and control handle: synchronized movement of two indexes

Optical Head : Detector

Optical encoder

Weight

Tester: Approx. 60 kg Control unit: Approx. 5 kg

*1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

Read more
Show Less

210

Loading Unit : Loading Method

Electromagnetic force

Indenter : Upper pressure indenter

Type: Flat indenter (50 µm diameter)
(500 µm flat indenter as option)
Material: Diamond

External Dimensions

Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

Utilities : Humidity

80% max. (no condensation)

Utilities : Vibration

Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
0.01 µm max. (at less than 10 Hz)
Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
0.005 µm max. (at less than 10 Hz)

Utilities : Temperature

Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

Utilities : Grounding*1

The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

Utilities : Power Consumption

Approx. 100 W (not including power consumption of PC)

Available test parameters : Power Supply

Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

Available test parameters : Data Processing Items

Calculation of compressive strength, display of test parameters and results
Display of test force and displacement data
Display of test force/displacement curve
Display of test force/displacement identification value
Display of strength/particle diameter curve
Display of displacement/time curve
Display of strength/parameter curve

Available test parameters : Shape of specimen

Particle, fiber or other shapes

Available test parameters : Test mode

Compression test, load-unload test, cyclic test

Specimen stage : Horizontal positioning range

25 mm for both X and Y directions
Min. increment: 0.01 mm (0.001 mm with option)

Specimen Stage : Area

Approx. W 125 mm × D 125 mm

Specimen stage : Vertical positioning range

Approx. 60 mm

Indenter : Lower pressure plate

SKS flat plate (Diamond pressure plate available as option)

Optical Head : Min. increment

0.01 µm / pulse

Loading unit : Loading range (mN)

9.8 – 1961

Optical monitor : Total magnification

Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

Loading unit : Load Accuracy

Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

Loading unit : Resolution (µm)

2 (when testing at 19 mN or less)

Displacement measurement unit : Method

Differential transformer

Displacement measurement unit : Measurement range (µm)

0 – 100

Displacement measurement unit : Min. increment (µm)

0.001

Displacement measurement unit : Linearity

Within ± 2% of full scale

Optical Monitor : Objective Lens

× 10, × 50 (× 20, × 40, × 100 with option)

Optical Head : Effective measurement range

Approx. 200 µm (with × 50 objective lens)

Optical Monitor : Eyepiece

× 10

Optical monitor : Illumination method

Epiluminescent

Optical monitor : Illumination lamp

LED 3 W / 3 V

Optical monitor : Light path

Switching between observation and photography possible

Optical Head : Collimation method

Direct connection between encorder and control handle: synchronized movement of two indexes

Optical Head : Detector

Optical encoder

Weight

Tester: Approx. 60 kg Control unit: Approx. 5 kg

*1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

Read more
Show Less

211

Loading Unit : Loading Method

Electromagnetic force

Indenter : Upper pressure indenter

Type: Flat indenter (50 µm diameter)
(500 µm flat indenter as option)
Material: Diamond

External Dimensions

Tester: Approx. W 355 × D 405 × H 530 mm Control unit: Approx. W 315 × D 375 × H 110 mm

Utilities : Humidity

80% max. (no condensation)

Utilities : Vibration

Horizontal vibration: 0.017 Gal max. (at 10 Hz or more)
0.01 µm max. (at less than 10 Hz)
Vertical vibration: 0.010 Gal max. (at 10 Hz or more)
0.005 µm max. (at less than 10 Hz)

Utilities : Temperature

Recommended temperature: 23 ± 1°C Allowable range: 10°C to 35°C

Utilities : Grounding*1

The grounding pins of 3-pin connectors must be connected to a resistance of 100 W or less.

Utilities : Power Consumption

Approx. 100 W (not including power consumption of PC)

Available test parameters : Power Supply

Single phase AC 100–115 V ± 10%, AC 230 V ± 10% (Ground resistance 100 Ω max.)

Available test parameters : Data Processing Items

Calculation of compressive strength, display of test parameters and results
Display of test force and displacement data
Display of test force/displacement curve
Display of test force/displacement identification value
Display of strength/particle diameter curve
Display of displacement/time curve
Display of strength/parameter curve

Available test parameters : Shape of specimen

Particle, fiber or other shapes

Available test parameters : Test mode

Compression test, load-unload test, cyclic test

Specimen stage : Horizontal positioning range

25 mm for both X and Y directions
Min. increment: 0.01 mm (0.001 mm with option)

Specimen Stage : Area

Approx. W 125 mm × D 125 mm

Specimen stage : Vertical positioning range

Approx. 60 mm

Indenter : Lower pressure plate

SKS flat plate (Diamond pressure plate available as option)

Optical Head : Min. increment

0.01 µm / pulse

Loading unit : Loading range (mN)

9.8 – 1961

Optical monitor : Total magnification

Approx. × 100, × 500 (× 200, × 400, × 1000 with option)

Loading unit : Load Accuracy

Within ± 1% of displayed test force or 0.1 mN (whichever is greater)

Loading unit : Resolution (µm)

2 (when testing at 19 mN or less)

Displacement measurement unit : Method

Differential transformer

Displacement measurement unit : Measurement range (µm)

0 – 10

Displacement measurement unit : Min. increment (µm)

0.0001

Displacement measurement unit : Linearity

Within ± 2% of full scale

Optical Monitor : Objective Lens

× 10, × 50 (× 20, × 40, × 100 with option)

Optical Head : Effective measurement range

Approx. 200 µm (with × 50 objective lens)

Optical Monitor : Eyepiece

× 10

Optical monitor : Illumination method

Epiluminescent

Optical monitor : Illumination lamp

LED 3 W / 3 V

Optical monitor : Light path

Switching between observation and photography possible

Optical Head : Collimation method

Direct connection between encorder and control handle: synchronized movement of two indexes

Optical Head : Detector

Optical encoder

Weight

Tester: Approx. 60 kg Control unit: Approx. 5 kg

*1 This product is a precision measuring device. Special consideration is required for the product's installation conditions.

Read more
Show Less

MCT Series

Required PC Specifications

OS

Windows 7 (32/64 bit edition)

CPU

1 GHz min.

Disk Drives

CD-ROM drive

Display Resolution

1024 × 768 min.

Expansion Bus

PCI Express ×1, 2 slots min.

Read more
Show Less

MCT-510

Loading Method

Electromagnetic loading method

Test force range (mN)

9.8 to 4903

Displacement measurement range (µm)

0 to 100

MCT-511

Loading Method

Electromagnetic loading method

Test force range (mN)

9.8 to 4903

Displacement measurement range (µm)

0 to 10

MCT-210

Loading Method

Electromagnetic loading method

Test force range (mN)

9.8 to 1961

Displacement measurement range (µm)

0 to 100

MCT-211

Loading Method

Electromagnetic loading method

Test force range (mN)

9.8 to 1961

Displacement measurement range (µm)

0 to 10