Compression Test Jig for Foam Rubber Specimens - Specs
Foam Hardness Measurement
The following shows the test control and data processing for obtaining foam hardness.
<Control pattern>

<Data processing>
- Hardness of specimen (specimen thickness at initial test force value)
- Hardness at 25 %, 40 % and 65 % of specimen thickness is obtained.
Compression Deflection
The following shows measurement of the compression deflection coefficient and hysteresis loss ratio of foam.
<Control pattern>

<Data processing>
- Compression deflection coefficient (S65/S25)
- Hysteresis loss (area enclosed by reciprocation/area of forward feed × 100)
Compression Test Jig for Foam Rubber Specimens
Max. test force |
1 kN |
---|---|
Plate dia. (mm) |
200 mm dia. |
Specimen support plate (mm) |
400 × 400 |
Specimen support plate air holes (mm) |
Dia. 6.5, center distance 20 |
Operational temp. range |
0 to +40 °C |