SIE-560

Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

Measurement range

Max. 560 mm

Measurement principle

High-precision magnetic induction linear sensor

Measurement precision

0.5 % or less or ±2.5 µm of indicated value, whichever is larger

Gauge length

10 mm to 550 mm

Compliant Standards

Plastics Tensile Testing Standard  ASTM D638
Metallic Materials Tensile Testing Standards
ISO 6892, JIS Z 2241, ASTM E8

Applicable Specimens

Steel, non-ferrous metals, composite materials (CFRP, GFRP, etc.), and general-purpose plastics

Read more
Show Less

SIE-560S

Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

Measurement range

Small range: Max. 4 mm
Large range: Max. 560 mm

Measurement principle

Small range: Ultra-high precision strain gauge type sensor
Large range: High-precision magnetic induction linear sensor

Measurement precision

0.5 % or less or ±1 µm of indicated value, whichever is larger

Gauge length

50 mm (can be optionally changed to 10 to 40 mm)

Compliant Standards

Plastics Tensile Testing Standard
ISO 527, JIS K 7171, ASTM D638
Metallic Materials Tensile Testing Standards
ISO 6892, JIS Z 2241, ASTM E8

Applicable Specimens

Steel, non-ferrous metals, composite materials (CFRP, GFRP, etc.), and general-purpose plastics

Read more
Show Less

SIE-560A

Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

Measurement range

Max. (560 - gauge length) (mm)

Measurement precision

± 1 µm, 0.5 % (JIS B7741 0.5 class)

Gauge length

10 to 550 mm

SIE-560SA

Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

Measurement range

Max. (560 - gauge length) (mm)

Measurement precision

± 1 µm, 0.5 % (JIS B7741 0.5 class)

Gauge length

50 mm (variable with option)

Downloads

Download the latest brochure.