Fully Automatic Rubber Tensile Testing System - Specs

Fully Automatic Rubber Tensile Testing System

Applicable specimen

JIS K6251 No.3 and No.5: For tensile testing
JIS K6252 Crescent type and angle type (optional)

Load capacity

1 kN

Test speed

5 to 500 mm/min

Grip, bending jig

1 kN pneumatic eccentric roller type grip

Gauge length extensometer

Contact type extensometer (GL20, 25 mm)

Specimen size measuring device

Linear gauge type

Specimen storage unit

Pallet type

Data processing unit

JIS K6250, 6251, 6252 (optional) compliant

Read more
Show Less

Fully Automatic Rubber Tensile Testing System

Load capacity

Max. 1 kN

Test speed

0.001 to 1,000 mm/min

Specimen storage method

Palette type (120 pcs)

Applicable standard

JIS K6251