AGX-10kNVD

Capacity

Table-top model 10N to 50kN

Testing speed

0.0005 to 3,000 mm/min

Test force measurement accuracy : High-accuracy type

Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Standard-accuracy type (Select one.)

Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating)

Read more
Show Less

AGX-20/50kNVD

Capacity

Table-top model 10N to 50kN, floor model 20kN to 600kN

Testing speed

0.0005 to 1,500 mm/min

Test force measurement accuracy : High-accuracy type

Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Wide ranging type

Accurate to within ±1 % of indicated test force (for forces ranging from 1/2000 to 1/1000 of the load cell capacity rating)
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Standard-accuracy type (Select one.)

Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating)

Read more
Show Less

AGX-20/50kNV, AGX-100kNV

Capacity

Table-top model 10N to 50kN, floor model 20kN to 600kN

Testing speed

0.00005 to 1,500 mm/min

Test force measurement accuracy : High-accuracy type

Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Wide ranging type

Accurate to within ±1 % of indicated test force (for forces ranging from 1/2000 to 1/1000 of the load cell capacity rating)
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Standard-accuracy type (Select one.)

Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating)

Read more
Show Less

AGX-250/300kNV

Capacity

Table-top model 10N to 50kN, floor model 20kN to 600kN

Testing speed

0.00005 to 720 mm/min

Test force measurement accuracy : High-accuracy type

Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Wide ranging type

Accurate to within ±1 % of indicated test force (for forces ranging from 1/2000 to 1/1000 of the load cell capacity rating)
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating)
Accurate to within ±0.3 % of indicated test force (for forces ranging from 1/100 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Standard-accuracy type (Select one.)

Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating)

Capacity

Table-top model 10N to 50kN, floor model 20kN to 600kN

Testing speed

0.00005 to 540 mm/min

Test force measurement accuracy : High-accuracy type

Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/500 to 1/1 of the load cell capacity rating)

Test force measurement accuracy : Standard-accuracy type (Select one.)

Accurate to within ±1 % of indicated test force (for forces ranging from 1/500 to 1/1 of the load cell capacity rating)