CFT-EX Series - Specs

Capillary Rheometer Flowtester

CFT-EX Series

Extrusion force

CFT-500EX: 0.4903 to 49.03 MPa (0.4903 MPa step)
CFT-100EX: 0.098 to 9.807 MPa (0.098 MPa step)

Test temperature

(Room temperature + 20) to 400 °C

Test type

Constant temperature tests, constant velocity rising temperature tests