AGX-V Series - Specs
AUTOGRRAPH Precision Universal Tester
AGX-10kNVD
Capacity |
Table-top model 10N to 50kN |
---|---|
Testing speed |
0.0005 to 3,000 mm/min |
Test force measurement accuracy : High-accuracy type |
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating) |
Test force measurement accuracy : Standard-accuracy type (Select one.) |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating) |
AGX-20/50kNVD
Capacity |
Table-top model 10N to 50kN, floor model 20kN to 600kN |
---|---|
Testing speed |
0.0005 to 1,500 mm/min |
Test force measurement accuracy : High-accuracy type |
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating) |
Test force measurement accuracy : Wide ranging type |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/2000 to 1/1000 of the load cell capacity rating) |
Test force measurement accuracy : Standard-accuracy type (Select one.) |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating) |
AGX-20/50kNV, AGX-100kNV
Capacity |
Table-top model 10N to 50kN, floor model 20kN to 600kN |
---|---|
Testing speed |
0.00005 to 1,500 mm/min |
Test force measurement accuracy : High-accuracy type |
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating) |
Test force measurement accuracy : Wide ranging type |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/2000 to 1/1000 of the load cell capacity rating) |
Test force measurement accuracy : Standard-accuracy type (Select one.) |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating) |
AGX-250/300kNV
Capacity |
Table-top model 10N to 50kN, floor model 20kN to 600kN |
---|---|
Testing speed |
0.00005 to 720 mm/min |
Test force measurement accuracy : High-accuracy type |
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/1000 to 1/100 of the load cell capacity rating) |
Test force measurement accuracy : Wide ranging type |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/2000 to 1/1000 of the load cell capacity rating) |
Test force measurement accuracy : Standard-accuracy type (Select one.) |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/1000 to 1/1 of the load cell capacity rating) |
Capacity |
Table-top model 10N to 50kN, floor model 20kN to 600kN |
Testing speed |
0.00005 to 540 mm/min |
Test force measurement accuracy : High-accuracy type |
Accurate to within ±0.5 % of indicated test force (for forces ranging from 1/500 to 1/1 of the load cell capacity rating) |
Test force measurement accuracy : Standard-accuracy type (Select one.) |
Accurate to within ±1 % of indicated test force (for forces ranging from 1/500 to 1/1 of the load cell capacity rating) |
Downloads
Download the latest brochure.