Large Sample Compartment - Specs

Large-Sample Compartments

MPC-603A Multi-Purpose Large-Sample Compartment

280 - Large Sample Compartment

This multi-purpose sample compartment allows measurement of various shaped samples to obtain both reflection and transmission spectra. An integrating sphere is built-in to ensure accurate measurement of solid samples.

- Original S-beam/R-beam switching function allows reflection measurement using incidence angles of 0 deg. for diffuse reflectance measurements and 8 deg. without leaning the sample for total reflectance measurements.

- The V-stage is sold separately. The sample position can be freely adjusted both forward and backward as well as up and down.

Wavelength range

220 to 2600 nm

Detectors

PMT, InGaAs, cooled PbS

Maximum sample size

Transmission 305 mm dia. x 50 mm thick
or 204 mm dia. x 300 mm thick
Reflection 305 mm dia. x 50 mm thick

Note 1: A separate space must be provided for the personal computer.
Note 2: A small tableFor the MPC-603A must be provided separate from that for the UV-3600 Plus series.
Table dimensions: Able to accommodate MPC-603A unit (W580 x D420 mm)
Table height: Within +8 to -15 mm of the UV-3600 Plus series table height

MPC-3100 Multi-Purpose Large-Sample Compartment

280 - Large Sample Compartment

Measurement wavelength range

240 to 2600 nm (MPC-3100)

Maximum sample size

Transmission: 305 mm dia. x 50 mm T or 204 mm dia. x 300 mm T
Reflection: 305 mm dia. x 50 mm T

For UV-3600 (MPC-3100)

MPC-2600A Multipurpose Sample Compartment

280 - Large Sample Compartment

Measurement wavelength range

220 to 1400 nm

Maximum sample size

Transmittance: 305 mm dia. x 50 mm T or 204 mm dia. x 300 mm
Reflectance: 305 mm dia. x 50 mm T

For UV-2600 series