SALD-201V - Specs
Laser Diffraction Particle Size Analyzer
Model-1
Method of measurement |
Laser diffraction method |
---|---|
Measuring range |
0.25-50μm* |
Optical system: Light source |
Semiconductor laser(670 nm in wavelength) |
Sample cell: Batch cell |
Pyrex glass and tetrafluoroethylene |
Power requirement: Analyzer main unit |
100,110,120,200,220 or 240VAC as ordered,100VA |
Power requirement: Analyzer main unit with CE mark |
100,115,230VAC,100VA |
Power requirement: Sampler with CE mark |
100,115,230VAC,100VA |
Dimensions and Weight: Analyzer main unit |
About 28cm wide,34cm deep 51cm high, and about 25kg in weight |
Environmental requirements: Temperature |
10-30°C |
Environmental requirements: Humidity |
20-80% |
PC hardware requirements |
IBM 100% compatible |
* Depends on the characteristics of the sample particles
Model-2
Method of measurement |
Laser diffraction method |
---|---|
Power requirement: Analyzer main unit with CE mark |
100,115,230VAC,100VA |
Environmental requirements: Humidity |
20-80% |
Environmental requirements: Temperature |
10-30°C |
Dimensions and Weight: Sampler |
About 24cm wide,33cm deep,29cm high,and about 11kg in weight |
Dimensions and Weight: Analyzer main unit |
About 28cm wide,34cm deep 51cm high, and about 25kg in weight |
Power requirement: Sampler with CE mark |
100,115,230VAC,100VA |
Power requirement: Sampler |
100,110,120,200,220, or 240VAC as ordered,100VA |
Power requirement: Analyzer main unit |
100,110,120,200,220 or 240VAC as ordered,100VA |
Measuring range |
0.25-350μm* |
Sampler: Material of wetted parts |
SUS304,silicone rubber,and polypropylene |
Sampler: Liquid pump |
Peristaltic pump,about 1,000cm3/min,in the maximum delivery rate |
Sampler: Sample bath |
SUS304 and about 200cm3 in capacity |
Sample cell: Flow-thru cell |
Fused silica,SU304,and tetrafluoroethylene |
Sample cell: Batch cell |
Pyrex glass and tetrafluoroethylene |
Optical system: Light source |
Semiconductor laser(670 nm in wavelength) |
PC hardware requirements |
IBM 100% compatible |