SALD-HC Series - Specs

High-Concentration Sample Measurement System

System Configuration/Accessories

System Configuration

 

  • Measurement holder for high-concentration sample ...... 2
  • CD-ROM (dedicated software*) ...... 1
  • Polarizing filter ...... 1
  • Glass slides ...... 1 box

  • * The dedicated software runs under the Windows95/98/Me/NT4.0/2000/XP OS.

 

Names of High-Concentration Sample Measurement Systems for SALD Series
Model Name Compatible Model
SALD-HC30 SALD-3101
SALD-HC22 SALD-2201
SALD-HC71 SALD-7101
SALD-301V-HC SALD-301V
SALD-201V ER-HC SALD-201V ER

Special Accessories

Glass sample plates created by forming shallow circular indentations in glass slides are available as special accessories.

This glass sample plate combined with a standard glass slide is effective in situations where the concentration is relatively low and merely enclosing the sample between two standard glass slides would make it impossible to attain sufficient diffracted/scattered light intensity.

The plates are available in six types, with indentation depths varying from 0.05 to 0.5 mm. They come in sets of 10 plates. A set consisting of two of each of the differing types (total 12 plates) also is available.

Name Indentation depth
Glass sample plate (0.1 mm) 0.1 mm (100 µm)
Glass sample plate (0.2 mm) 0.2 mm (200 µm)
Glass sample plate (0.3 mm) 0.3 mm (300 µm)
Glass sample plate (0.4 mm) 0.4 mm (400 µm)
Glass sample plate (0.5 mm) 0.5 mm (500 µm)
Glass sample plate (0.05 mm) 0.05 mm (50 µm)
Glass sample plate set 0.05 to 0.5 mm

* Appearance and specifications are subject to change without notice.