IG-1000 - Specs

Single Nano Particle Size Analyzer

IG-1000 Plus

Measurement principle

Induced grating (IG) method

Measurement range

0.5 to 200 nm

Measurement Time

30 sec (from the start of measurement to the display of results)

Sample Liquid Volume

250 to 300 µL

Measurement Unit: Light Source

Semiconductor laser (wavelength: 785 nm; output: 3 mW)

Measurement Unit: Light-receiving Unit

Photodiode

Measurement Unit: Cell

Batch cell (material: Pyrex glass*1)

Output Terminal

Serial output (connector type: D-Sub, 25 pin, female)

Temperature Setting Range

7°C to 40°C (cell holder temperature setting range*2)

Operating Environment

Temperature: 15°C to 35°C

Humidity: 20% to 80% (without condensation)

Humidity: 20% to 80% (without condensation)

Power supply

AC 115 or 230 V ±10%

Size and weight

600 (W) x 400 (D) x 200 (H) mm, approx. 15 kg

*1: Do not use the kind of solvents that may damage Pyrex glass.
* : Measurement is possible as long as the conductivity of the sample liquid does not exceed 400 μS/cm (microsiemens per centimeter). (For example, saline and seawater cannot be used for measurement unless they are greatly diluted.)

Read more
Show Less

IG-1000 Plus

Measurement range

0.5 to 200 nm

Measurement Time

30 sec

Batch cell method, sample volume

250 to 300 µL

Downloads

Download the latest brochure.