Application
News
www.shimadzu.com/an/
Shimadzu Corporation
© Shimadzu Corporation, 2023
For Research Use Only. Not for use in diagnostic procedures.
This publication may contain references to products that are not available in your country. Please contact us to check the availability of these
products in your country.
The content of this publication shall not be reproduced, altered or sold for any commercial purpose without the written approval of Shimadzu.
See http://www.shimadzu.com/about/trademarks/index.html for details.
Third party trademarks and trade names may be used in this publication to refer to either the entities or their products/services, whether or not
they are used with trademark symbol “TM” or “”.
Shimadzu disclaims any proprietary interest in trademarks and trade names other than its own.
The information contained herein is provided to you "as is" without warranty of any kind including without limitation warranties as to its
accuracy or completeness. Shimadzu does not assume any responsibility or liability for any damage, whether direct or indirect, relating to the
use of this publication. This publication is based upon the information available to Shimadzu on or before the date of publication, and subject
to change without notice.
First Edition: Dec. 2023 01-00647A-EN
Conclusion
Nexera and Shim-pack are trademarks of Shimadzu Corporation or its affiliated companies in Japan and/or other countries.
In this article, an on-line dissolution test of loxoprofen sodium
tablets using Nexera FV has been reported. The fraction analysis
mode allows 5-minute sampling interval. The direct injection
analysis mode doesn’t require preparing vials for fractionation
resulting in cost reduction. Thus, Nexera FV is an on-line HPLC
system setup that can provide automated and efficient
dissolution testing for drug products.
Table 2 HPLC analytical conditions
Column : Shim-pack XR-ODSⅡ
*1
(
75 mm
×
3.0 mm I.D., 2.2 µm
)
Mobile phase : Methanol/Water/Acetic Acid/Triethylamine
=600 : 400 : 1 : 1
Flow rate : 0.8 mL/min
Column temp. : 40 ℃
Injection vol. : 2 µL
Detection : UV 222 nm
*1 P/N:228-41624-91
● Analysis of standard solution
Using a 1.5 mL ordinary vial, six repeated analyses of a standard
solution of loxoprofen sodium (60 mg/L) were performed. Fig. 5
shows the chromatograms and Table 3 shows the results. Good
results of around 0.05% RSD for both retention time and peak
area values were obtained.
0.00 0.50 1.00 min
0
100
mAU
Loxoprofen Sodium
Fig.5 Chromatogram of standard solution of loxoprofen sodium (60 mg/L)
Retention time
(min)
Area
1st 1.051 248,209
2nd 1.052 248,265
3rd 1.053 248,129
4th 1.052 248,232
5th 1.052 248,380
6th 1.051 248,038
Averages 1.052 248,209
%RSD 0.07 0.05
Table 3 Retention Time repeatability and peak area repeatability
for a standard solution (60 mg/L、n=6)
● Fraction analysis mode
The test solutions were sampled six times at 5, 10, 15, 20, 25,
and 30 minutes. Fig. 6 shows the chromatogram of the test
solution loxoprofen sodium tablet (68.1 mg per tablet indicated,
dissolution time; 30 minutes).
Loxoprofen Sodium
0.00 0.50 1.00 min
-100
0
100
mAU
Fig.6 Chromatogram of test solution of loxoprofen sodium tablet (dissolution
time; 30 min)
Table 4 shows the time-dependent variation of the dissolution
rate in each vessel, and Fig. 7 shows the dissolution curve of
loxoprofen sodium tablets.
The Japanese Pharmacopoeia, as ascribed, specifies that the
dissolution rate of loxoprofen sodium tablets must be at least
85% in 30 minutes, and the results obtained from this study met
this criterion.
Table 4 Time-dependent variation of dissolution rate in each vessel (%)
Time
(min)
Vessel No.
5 10 15 20 25 30
1 26.28 62.34 85.67 98.45 99.53 99.49
2 23.88 59.71 84.98 99.07 101.08 100.89
3 23.90 58.78 86.68 99.80 101.27 101.18
4 24.33 56.44 83.55 98.18 100.25 100.64
5 23.54 59.62 84.81 98.77 100.54 100.61
6 24.77 59.54 85.97 100.41 101.15 101.59
Vessel No.
Fig.7 Dissolution curves
Dissolution time (min)
Dissolution rate* (%)
*:Dissolution rate(%)=Concentration(mg/L)×Media Volume 0.9(L)/Labeled amount 68.1(mg)×100
● Direct injection analysis mode
Then, on-line dissolution test in direct injection analysis mode
was performed. The test solutions from six vessels were
sampled at 30 minutes only. Table 5 shows the dissolution rate
in each vessel. In direct injection analysis mode, each
dissolution rate 30 minutes was over 85%, which met the
criterion as well.
Time(min)
Vessel No.
30
1 103.49
2 101.67
3 100.40
4 100.29
5 102.42
6 102.32
Table 5 Dissolution rate (%) in each vessel